Viscosity changes are not always evidence of defective material. Temperature, heating duration, oxidation, contamination, formulation characteristics, and measuring methods can all alter how a hot melt adhesive flows. The key production question is whether the change remains within a controlled operating range or signals degradation that could affect coating weight, wetting, and bond consistency.